Proper Gash & Web Thickness on a Carbide End Mill

How to spot a proper End Mill GASH & WEB Thickness:

First let’s go into a little bit of detail on exactly what we are referring to. During the manufacturing of an end mill there are various operations that create the necessary geometries which produce the final product. In this example we are teaching about Gash and Web Thickness. Without careful attention during the manufacturing process this is an area of the end mill that can easily be out of spec resulting in poor tool performance.

The Gash is the “operation of removing material” to create the Web Thickness along the very top of the tool. The Web thickness is the end result. Shown below on a 2FL End Mill (top view) it is the area in Yellow (gash) where it meets the thinnest point of the area in blue (web thickness result).

End Mill GASH

Proper Gash & Web Thickness:

The photo to the left shows an End Mill with Proper Gash and Web thickness. You’ll notice that the primary clearance intersects to a minimal point.

The exact ideal measurement of the web thickness will depend on the diameter of the end mill itself.

 

 

 

 

 

Gash too far behind center 6_6

Improper Gash & Web Thickness:

This example demonstrates and End Mill with the gash being too far behind center causing the web thickness to be non-existent.

Results: This can cause the tool to be weak and break during operation.

 

 

 

 

 

Gash too far ahead of center 6_6

Improper Gash & Web Thickness:

This example demonstrates an End Mill with the gash being too far ahead of center causing the web thickness to be too large.

Results: This creates an area along the end of the end mill that will not cut. This causes the end mill to work harder, requiring more CNC machining power. In an end cutting milling operation the tool will act dull even if it’s not.

 

 

Share

Speak Your Mind

*